Sunday, October 17, 2010

Count Down Fun! 3! Part 3 ~ Picture Heavy Sorta Word Light

It was so cool this morning that I couldn't invest until 2 PM.  That meant the flask went into the kiln, for an 8 hour burnout cycle, at 3:15 this afternoon . . .  I poured at 12:30 tonight.  The trees are devesting in a sealed jar of plain water in the ultrasound right now.  I'll switch them into pickle before I go to bed.  So far they look good, we'll know for sure when they come out of the pickle tomorrow.

So here's some more of what we did today . . .  Besides the major pendants that Pat finished, she also worked on our new Seasonal Botanical Earrings!

Jump rings soldered on, textured freshly patinated.

 Detail texturing the ends after patinating.
Pat:  "You know, if we do these the way we want to we're not charging enough."
Tom:  "Yeah, I know."

I wonder what we'll do with this newly cast Bronze Fern . . . ? 

While I was minding the kiln I was shooting waxes for our production earrings.
This is what the wax injector looks like after a couple of days of hard work! 

I talked about making and cutting molds way back here if you're curious.

When I'm doing production work I like to shoot six molds at a time.  That way the first will be cooled enough to "pull" the wax by the time I've shot the last.  I hold the mold between two sheets of thick aluminum and press them against the injectors nozzle.  For this wax, MagnaJect Pink, the wax pot is running a little over 150 F.  With the pressure gauge generally at 3 to 3.5 psi most molds take a count of ten to fill well.  Some molds take a bit longer ~ you learn how your molds shot and adjust accordingly.

Here's how you pull a wax . . .

Every mold has a top and a bottom, lift the top off. 
Use a long thumbnail to cut the sprue free. 

Flex the mold to free the wax and lift it out.

Check for air bubbles and any incomplete details. 
Shot the now empty mold again.

Repeat until you're done!  Make some extras just to be sure.

I'm always working with my master shooting list beside me, so I can keep track of what I'm working on:  how many we'd like to have of what designs, variations and combinations.  (At last count I've come up with 72 different variations of our production Ridgelines earrings already, and we have more shapes still to come!)

Last weekend I talked about how and why I make wax jump rings back here.
Now it's time to use more of them!

For me the key to production work is to be efficient, fast and always do it right.
Working on the same step of multiple pieces helps.
4 pairs of small oval Ridgelines ready to go

The jump ring is glued in place with the cut at the bottom,
checked for centering and balance

from both sides and from above. 
I know it looks a little cockeyed.  It isn't, the sprue isn't centered.
Repeat until done.

When the jump rings are glued it's time to lute them ~ to seal them in place with wax.

I use my Dual Therm wax pen's finest tip to apply low melting point red sprue wax to both sides of the jump ring, making sure to get inside the lower area to ensure where the coil was originally cut is completely closed. 
Repeat until done.

Tonight I stopped at 7, turned the kiln to High and made a quick and easy dinner.  It took a little longer than I had expected, but it was good.  We spent a little time relaxing together.  Then I got back to work.  I want to get two more trees of waxes sprued for tomorrow!

But as soon as I sat down in the office I got mugged by Inky!!!

"Daaad.  You haven't really cuddled me allll day . . ."

"Are we reaally going to work, right nooow???"

"I didn't think so!"

"Oh that's good."

"Watdaya mean enough?!"

"Oh, oh, oh.  Right there, right there!"


After we both had a good cuddle love session I was able to sprue up the first tree of waxes for tomorrow.  Someday some very lucky person is going to fall in love with a pair of our Ridgelines earrings and they'll never know that Inky helped make them!

By the time I got the second batch glued and ready to lute it was time to turn all of my attention to the kiln and weigh out my metal (Flask #1 82 g., Flask #2 92 g.) and get ready to cast.

I have one tree ready for tomorrow.  At this point the other waxes won't take me too long to sprue up.  I could have kept going for a little while, but posting this has been a nice way to wind down and end the evening.

Our chains are supposed to be in from Italy Monday.  As long as they're here by Wednesday we'll be very happy!

And I just know there's something I've forgotten that I really should remember to write down.  I wonder what  .  .  . ?

Oh.

I need to take a shower!  And I should do some laundry when I have a chance . . .

Friday, October 15, 2010

Count Down Fun! 5! Part 2, "You know . . ."

[I just discovered that this was saved as a draft last night when I fell asleep in my office chair!  So here's yesterday's second post ~ please just ignore any confusing tense usages and pretend that you're reading it yesterday  .  .  . ]

You know, there's a reason that casting is as much an art form as it is a science . . .

Pat test wearing our newest
Seasonal Botanicals in Sterling Silver !!!

This is another case of taking a break outside and really looking at the wonderful world around us.  I saw this amazing shape and knew that I just had to see what they would look like, and feel like, what they would be as a piece of jewelry.  How could anyone possibly improve on this form, this shape, these proportions???  You can't.

This is one of the first pairs of earrings that I had to try to cast (I think it was) last week (?) because of this inspiration.  (The days are beginning to blend together a little!)  And yes, if you saw my last post, these are actually seed pods from our Ipomoea guamoclit, or Hummingbird Vine.  These beautiful earrings began life as this beautiful flower:

Hummingbird Vine, also known as Star Glory or Cyprus Vine,
Ipomoea guamoclit.

Talk about a stretch your limits challenge!  The first test casting went well and I learned a number of things.  There was no way I could stop with just a couple.  So I had to make more!  But the clock is steadily ticking away and I just don't have time for experimenting ~ if something doesn't work the time and energy and effort is gone.  (But not wasted!  Sometime we have to learn certain lessons more than once . . .)

It was disappointing to take Tuesday night's castings out of the ultrasound and think I'd found shrinkage porosity last night.  I used a miniature cut off disc to desprue the castings today.  And I feel alot better.  Only a couple actually suffered from shrinkage porosity!  (Generally caused by too small a sprue supplying too little metal to too large a mass.  Which was exactly what happened here.)  The rest are perfect and we'll have them at the Guild Fair!  (Providing we find the time to get them all finished!)  I got them all de-sprued and rough ground for Pat today.  She finished up the forged rings so I've got them waiting in the que for grinding and buffing and final polishing.

Between our long dry spell and the cold nights we're having now these might just be the only Hummingbird Vine castings I can make this year.

Our chains haven't arrived from Italy yet, so I called today.  They should be here today or tomorrow.  As long as we have them by next Wednesday we'll be happy.

While I was minding the kiln today Pat got lots more finished up than I did.  Thank goodness!  (Why, oh why, do I still think I can get a dozen other things done when I'm casting???)

Ferns, waxed and ready for spruing*.

So I made dinner a little later than I probably should have tonight.  Pat offered to, but I was already so hungry-wired that I just wasn't being effective so it was better for me to stop working and get into the kitchen.  I made Pat flop on the couch with a good book.

So we ate and then I cast the Ferns at 7:27 tonight.  It was 56 degrees out, though because the kiln and Electro-Melt were running it was 65 in my casting area.  I charged the Electro-Melt with 59 grams (just a smidge under 2 ounces) of Everdur Silicon Bronze once it was preheated to 1850 degrees Fahrenheit.  The kiln and flask were at 950 degrees F.  Normally I'd cast Silicon Bronze with the flask at 900, but it was a cool evening and the ferns are delicate finely detailed pieces.  (Remember that:  "Delicate finely detailed pieces" . . .)

Here's tonight's 1 minute 30 second video of the pour.  If you want to skip ahead to see the four seconds it takes to pour 2 ounces of molten metal, the Fun Part starts at 54 seconds.  This is the make or break point of more than two very full very long days of work and another day spent burning out the flask . . .


Ten minutes later, because it was so cool, the button wasn't glowing and it was time to quench.  And I immediately knew I had problems.  Despite the extremely excessive spruing three of the five ferns completely failed to cast . . .

Gut-dropping, stomped flat, sick to the stomach about sums up how I felt when I first held the castings in my hand.  What ???  Sure, we all know ferns are too thin and too light to cast.  But I've done 'em before and . . .

When I first started casting [lets be polite and just say it was a couple of decades ago, okay?] everything that could go wrong did.  There are so many things that have to be just right to making a casting work, or not, that sometimes I couldn't figure out what had happened!  I wish I could find it now but, I wrote out a list of every single step involved and what might go wrong if you made a mistake at any step and what the affects would be on the casting.  For some reason the number 311 still jumps into my mind all these years later.  (It might've been 315.)

So by my, ancient, calculations from the wax stage to the final quench there are more than 300 hundred ways that you can completely mess up a casting . . .

But more importantly, just what the heck went wrong this time?!?  And how the heck have I messed up two castings in a row???  Am I really that tired???

The metal temp was at 1950 when I poured.  Silicon Bronze is, like DeOxidized Sterling Silver, kind of funny stuff to melt.  There's the melting point of the metal and then there's the liquidous point ~ and sometimes there's another altogether different temperature for the pouring point.  When Silicon Bronze first melts it looks like an antique mirror with a crackly crazzed surface; raise the temperature another 20 or 25 degrees and that affect disappears as the silicon is activated and you're good to pour.

Okay.  It looked good or I wouldn't've poured when I did.  But my first suspicion was the metal's temperature and even though I tried to allow for the ambient temperature that's where I looked first . . . 

Oh.

Here's what I forgot to allow for!!!  Yep, I poured at the correct temperature ~ for a dense heavy casting.  For light delicate ferns I should have poured when the Bronze was another 50 to 100 degrees higher!!!

There's nothing to do but make a note in my casting log and hope that I'll always remember to double-check in the future.  Then you turn the music on and smile and dance.

It's such a Beautiful World and there is always more to remember and to learn. 

So if that was the problem why did I say casting is as much an Art as it is a Science???

Because if I had listened to, and really heard, my own inner voice saying, "Um, it's not hot enough yet . . ." regardless of what the pyrometer said, I think they would have all turned out perfectly.

I didn't listen.  Now all I can do is dance and smile and laugh with the music.

If today is suddenly Friday it must be time for lists, or maybe it's time for bed   .   .   .

Sam & Ink again, late this July, just because.

*Gee, aother word that I seem to automatically misspell!  Sprueing should be spruing.  Though ti, er, it makes me feel better to see how many people have googled sprueing and landed on our blog!

Thursday, October 14, 2010

Count Down Fun! 7! 6!! Catching Up, I Hope . . .

This is the morning of Count Down Fun Day 5, as I try catch you up on what we did on Days 7 & 6.  (Lets see if the video works!)

Last time I talked about investing the new Seasonal Botanicals.  On Day 7 they went into the preheated kiln at 300 F at 10 AM.  I spent the day waxing new Fern Seasonal Botanicals.  And waxing, and waxing, and minding the kiln.

It was a pretty well behaved burnout cycle.  There's always a lag between the kiln temperature and the actual temperature of the flask being burned out.  Especially at the lower temperatures, but once the water content has been forced out by the heat and you reach the 1000 degree point the flasks tend to be pretty responsive to temperature changes.  (Though just because of their size and weight there is still a bit of a lag in temperature changes.)  Anyway . . .

Because of the time/temperature lag I start counting down each stage of the burnout cycle once the kiln actually reaches the new temperature range.  For example, the main high temperature for a 3" by 3" flask is 1350 degrees F for three hours.  So when I go from the 2nd stage at 700 F I don't begin timing until the kiln is actually at 1350 F.  And that's the fiddly stage for my old electric kiln.  (An American Ceramics kiln that I dearly love and owe an awful lot to.)  An hour and a half into the 1350 F stage I'll pull the flask, rotate it approximately 90 degrees and turn it over so the sprue former pour cup is now facing up.  Then back in, make sure it's at 1350 F and time for another hour and a half.

The actual pour was at 6:30 PM.  Wait about 15 minutes to let the flask cool then quench.  Then you finally get an idea if all of the wax work and then the burnout and pour worked.

I don't have a way to edit video yet, so this 3 minute clip is a bit rough.  I tried setting the camera up facing my casting area.  From the camera what you see is:  my Vic 9 vacuum caster, my Kerr Maxi Electro-Melt  (100 oz capacity!), and behind that the side of the kiln.  The very loud noise you hear is the exhaust fan.  The even louder noise later is the vacuum caster when it's turned on.  It's dark, but wait till you see the molten metal flowing!!!

Here's a quick timeline:

.10 Charging the Maxi-Melt with 90 grams of Sterling Silver (3 oz) when it is at 1850 F
.30-.40 Rocking the Maxi-Melt to help mix the alloy and sometimes, if it's a lot of metal I can feel if it has begun to melt
.50 checking the melt. Nope, not ready.
1.40+ rocking the Maxi-Melt, feels good, lets check it!
1.50 quick stir with my quartz stirring rod to make sure the melt is complete & to mix it
2.04+ turn off the kiln, pull the flask and set it on the casting table, turn on the vacuum pump and check the vacuum gauge to make sure the flask is drawing a vacuum
2.19 the beginning of the pour & my very favorite part of casting. All the hours and days of work lead up to the next few seconds.

After the actual pour I dump any residual slag out onto my fire resistant base and make sure the graphite crucible is clean. Turn off the Maxi-Melt and unplug it.



The last bit is jumpy because I wanted to show what the flask looks like from my view as it is glowing at me.  Sorry 'bout that, but after the Fair I'll have time to work on editing some more videos.

After cooling a bit I quenched then put it into a glass jar to devest in the ultrasound.  Made dinner and we both decided that we were pretty much done for the evening.  Around midnight I transferred these castings to a pickle jar and left them in the ultrasound for the night.  I turned the ultrasound off when I went to bed around 2.

Just as a reminder, there's a reason I look like this when I'm casting!!!
  • Full respirator ~ don't want to breath in any metal fumes!
  • Casting glasses ~ I'm looking directly at and into 1850+ degrees F!
  • Welding glove on my right hand ~ I use tongs to pull the flask out of a 1000 degree F kiln, and then I use my quartz rod to stabilize the 1850 degree F graphite crucible as I pour.
Yesterday, Day 6 I spent working on new Fern Botanicals.  And working on them, and working on them.  I have to admit I was in a groove and loving it.  They came along really well, but took a lot longer than I had meant them to.  (I thought I'd get them burned out and cast yesterday.  HA!  I just kept working on them.)  I left the earlier Botanicals in the ultrasound all day.  Just got distracted and left them running in fresh water.

Pat got a lot done on the production earrings for the spinner rack over the last few days.  Yesterday she finished the larger pendants that had been on the bench.

We stopped and I made us dinner around 7:30.  Then I went back to working on the Ferns.  I pulled the castings and dried them off . . .

And that was when I finally saw that some of them had shrinkage porosity and aren't usable.  Blankity-blank-blank-blank!!!  It was my own fault.  So there's nothing to do at this point except make a note in my casting log and remember to have a heavier sprue the next time . . .

So, of course, I stayed in the office working on the Ferns and boy did I overcompensate!  I began to actually spruesprue them up ~ after I completely over did their sprueing!  There is no way they will have any shrinkage porosity.

But what a pain they're going to be when it's time to de-sprue them . . .

So now it's the morning of Count Down Day 5!  In four days I'll be loading the display in the car.  In five days we'll be setting up at Booth #109 in the arena level of the Asheville Civic Center.  In six days the Fair will open at 10 AM and we'll be there, all set up and ready to go!

Counting the days  .  .  .



Sunday, March 14, 2010

Last Night's Castings & No Email . . .

I put both flasks in the pre-heated kiln at 10 yesterday morning.  I expected my burnout cycle to take 7 hours, but ended up pouring just after 9 hours.  The weather turned a little colder and rainy so I had some heat lags to take into account.  It's better to be slow and sure, 'cause you can definitely run a burnout cycle too fast and too hot.

As I was pouring I could hear the first spring peepers calling nearby.  Spring really is coming!

A.'s Anniversary Brooch turned out beautifully!
I'll be spending quite a bit of time de-sprueing with mini-cutoff discs tomorrow.  But all those heavy sprues were worth it.  After I grind and polish Pat will be setting a 2.5 mm AA ruby into each of the 10 petals.  This is going to be a really lovely brooch!

The ring for The Jewelers Workbench turned out well too.

I've already de-sprued and ground it.  It needs a little touching up and a final polish and it will be ready to deliver tomorrow!

For some reason Earthlink's email has been out of whack all weekend.  We can't access our mail at all.  All their support has said since yesterday is, "We are currently experiencing high call volume indicative of an email outage. We are currently investigating further and apologize for the inconvenience. Please continue to check this site for updates."  Jeepers.

Our Dear Friend Greylond called us last night.  He's in the wilds of Mississippi.  He was sitting by his campfire enjoying a glass of wine and thinking of us.  I was having a glass of beer and had just thought of him shortly before he called.  We had a good long talk, about many things.  We each raised a glass, "To absent Friends!"

Monday, February 22, 2010

J.T.'s Earrings and Commissions

We had wonderful weather over the weekend!  It actually hit 62 Sunday and we were able to spend a little bit of time outside, once we finished up some work.  Here are the earrings that Pat finished for J.T. . . .
They are oxidized Sterling Silver with Niobium wire wrapped around the dangle as a nice color accent. with four prong mounted Garnets.

As I was photographing them this morning A.P. came by with a deposit for his commission.  It's an interesting one!  (And is an example of how time flys!)  Ten years ago we made their wedding bands.  Five years ago he had us make his Fifth Wedding Anniversary gift for her.  And now we are making his Tenth Wedding Anniversary Gift!

Here are the initial designs Pat skectched after we first spoke with him.  He decided on design number 8, with 10 2.5 mm Rubies in Sterling Silver.  It's going to be a lovely brooch!


Now, I have to get back to minding the kiln!  With this warmer weather I have to use every chance I have to get some castings done!  Right now I have the two flasks in that have been waiting so long.  I'm looking forward to seeing them in metal!  These pieces will be some of the first for our new River Ridgelines series and I'll be casting them in Silicon Bronze.

I have at least one more commission piece to cast and finish before next Monday.  Since the Guild's Board meeting is tomorrow and I'll be at an all day Fair Committee meeting (as the Board's Rep) Wednesday I won't have a chance to even think about casting again until Friday!

Time sure flys when you're having Fun !!!

Thursday, September 3, 2009

Friday (posted much later)


Sterling castings fresh out of the pickle. B's custom order is in the middle. Tom de-sprued these then ground and buffed B's ring before it went to Pat for sizing and mouting the peridot. Then Tom did the final buffing when he buffed the two custom gold wedding bands.










The big flask went into the kiln at 9 AM, right as the kiln had warmed to 300 F. This one will be an eight hour burnout cycle because of the size of the flask.


The custom gold rings are ready for their final buffing!





This is a quick sketch that Pat did from a customer's description. Tis is going to be a "fun" job: she wants her individual bracelets rounded, soldered together and then two pairs of lapis earring converted and soldered to the top of her new bangle bracelet.



Four pairs of locking tweezers being used to hold the ends in place for the first solder. (We've already discovered that one of her bracelets isn't usable, since it's hollow and filled with pitch. So we can't apply any heat to it.)







Making the first solder. We're going to have to start at one end and join the individuals bracelets together, then attach them as we go. Most of these bracelets are all different sizes too, so they'll have to be shortened as well.












Just as Pat was ready to bezel-set the peridot in B's ring she got mugged!







Sam said it was break time and he needed a cuddle right now!



You just have to take a minute and smile, and give him a good cuddle-love!













Then you can get back to work.

















From the customers' sketch of what they wanted their wedding bands to look like.




Pat took this photo years ago.  She referred to it when she was carving the waxes to help her visualize the mountains' contours, layering and textures.








The waxes the customer's approved . . .












To their wedding bands made real! 14 karat yellow gold with bezel-set sapphires.





The interiors, showing the open bezels.






Meanwhile Tom's been working waxes and minding the kiln.  Halfway through the heat soak stage, after turning the flask right-side up (what was the bottom, with the pouring cup and gate area now pointing upwards) at 4 PM the kiln ramped it's temperature up to 1450 F !!! Which is not good!

Investment is a special plaster mixed with water used for lost wax casting. It's funny stuff. It's delicate and fragile stuff, and it has to be heated slowly to drive the moisture off without causing steam and cracking it. The wax originals have to be melted out, the wax tray removed, and then the wax residue is literally burned out. Once investment has been heated to 1000 F it's pretty tough and the temperature can be quickly run up to 1350 F for the final burnout before it's lowered to whatever temperature the flask and metal will need for the actual casting.

Unfortunately though extended temperatures over 1375 F (or 1450 F depending on the investment) causes investment to break down! Fortunately for us, Tom caught the temperature pretty quickly ~ it had only run up to 1450 for a few minutes and there is always a fairly considerable lag betweent he kiln temperature at that of the flask, especially with a 3" X 5" flask like this one.

Still, it was an exciting moment when he checked the kiln temperature!

Pat left to make a delivery. Tom poured at 5:45 PM.
This is a view of the top of the flask right after casting. It's still sitting on top of the vacuum chamber (the other end of the flask is open and the gasses are drawn away through the investment as the metal flows in, hence vacuum-assisted casting).


Then Tom started a vegetarian spaghetti sauce before it was time to quench. This sterling alloy really does best if it is allowed to really cool, otherwise you can have heat-stress fractures which is never good ~ especially when you have so much time and work tied up in one flask!
The quench went well and Pat got home in time for a good dinner. Tom's Friend John came over for a Boys' Night and Pat deservedly loafed and watched a couple of videos.
Tom actually loves his old Kerr Maxi-Electro Melt. (Think of it as a glorified coffee pot for melting metals!) This one is an older, but large capacity, one that we bought second-hand from another Jeweler many years ago. He has a different graphite crucible for each metal that we cast (gold, silver, and bronze).
Here's what the crucible looks right after a pour. It's at 1850+ degrees Farenheit and it really glows!











Now, if all went well, I may have actually gotten this post from last Friday to upload correctly!!!